Synthesizing nano LaAlO3 powders via co-precipitation method

  • W. Li*
  • , M. W. Zhuo
  • , J. L. Shi
  • *此作品的通讯作者
  • CAS - Shanghai Institute of Ceramics

科研成果: 期刊稿件文章同行评审

摘要

Co-preparation method has been applied to synthesize nano LaAlO 3 powders. By using La(NO3)3 and Al(NO 3)3 as raw materials and keeping the pH ≈ 9, the co-preparation process could be finished at room temperature. Pure LaAlO 3 nano powders with a size of about 50 nm could be obtained after calcining at 700-800 °C. These nano LaAlO3 powders could be sintered at 1550 °C for 4 h, a high relative density of about 97% could be reached.