摘要
The Li 2SiO 3 powder has been successfully synthesized at low temperature via mechanical milling process. By using LiOH·H 2O and tetraethyl orthosilicate (TEOS) as raw materials, Li 2SiO 3 powder with grain size of about 100 nm could be obtained at room temperature (∼20°C) after mechanical milling for 120 h. This nano Li 2SiO 3 powder shows excellent thermal stability that no decomposing reaction or phase change would happen even after calcined at 900°C for 4 h. Experiments show that high concentration of the raw materials is helpful to the forming of Li 2SiO 3 phase. When the concentration of the raw materials is too low, no Li 2SiO 3 phase could be obtained. The investigation also shows that small content of B 2O 3 could accelerate the densifying speed of Li 2SiO 3 ceramics and decrease the thermal stability of Li 2SiO 3 phase.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 1818-1821 |
| 页数 | 4 |
| 期刊 | Journal of the American Ceramic Society |
| 卷 | 95 |
| 期 | 6 |
| DOI | |
| 出版状态 | 已出版 - 6月 2012 |
| 已对外发布 | 是 |
指纹
探究 'Synthesis of lithium metasilicate powders at low temperature via mechanical milling' 的科研主题。它们共同构成独一无二的指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver