摘要
The corrosion mechanism of municipal solid waste incineration (MSWI) fly ash on magnesia-chromium refractories from the perspective of substance migration and transformation was investigated by using corrosion test at 1400 ℃. XRD, XRF, and SEM-EBSD characterization and thermodynamic software FactSage analysis were utilized. Although thermally stable compound MgCr2O4 can be formed in the refractories mitigating the corrosion, the SiO2 in the fly ash can convert MgCr2O4 to Mg2SiO4 (forsterite) and MgSiO3.The regeneration and transformation of MgCr2O4, as well as the low melting point and volume expansion properties of Mg2SiO4 and MgSiO3, are responsible for the loosening of the refractory structure and the migration of magnesium from the refractory into the ash. When the refractory was corroded by MSWI fly ash repeatedly, the migration of the corrosion products from the refractory to the ash was the key to aggravate the corrosion. Increasing CaO content can mitigate the corrosion and magnesium migration by alleviating the formation of Mg2SiO4 and MgSiO3.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 1811-1821 |
| 页数 | 11 |
| 期刊 | Journal of the Australian Ceramic Society |
| 卷 | 61 |
| 期 | 5 |
| DOI | |
| 出版状态 | 已出版 - 12月 2025 |
联合国可持续发展目标
此成果有助于实现下列可持续发展目标:
-
可持续发展目标 11 可持续城市和社区
-
可持续发展目标 12 负责任消费和生产
学术指纹
探究 'Substance migration and transformation during the corrosion of magnesia-chromium refractories by municipal solid waste incineration (MSWI) fly ash' 的科研主题。它们共同构成独一无二的学术指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver