摘要
Hexagonal GeO2 ceramic films were fabricated at room temperature via an acid induced liquid phase deposition (LPD) method. Thick GeO2 glass films were prepared using a melting and quick cooling technique. The glass films were annealed in a mixed hydrogen/nitrogen gas atmosphere to create more oxygen vacancies. The intensity of 5-eV absorption band enhances with increase of annealing temperature as well as time. The activation energy of oxygen vacancy formation is calculated to be 0.91 ± 0.05 eV. The 5-eV absorption band is photobleachable, and the saturated absorptivity change reaches 575 ± 17 cm- 1.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 2884-2888 |
| 页数 | 5 |
| 期刊 | Journal of Non-Crystalline Solids |
| 卷 | 356 |
| 期 | 50-51 |
| DOI | |
| 出版状态 | 已出版 - 11月 2010 |