摘要
In this study, a microfibrous carrier consisting of 3 vol.% of 8 μm (diameter) glass fibers is used to entrap 45 vol.% of 150 to 250 μm (diameter) SiO 2, support particulates. ZnO is then nanodispersed onto the support by impregnation at the loading of 17 wt.%. At equivalent bed volumes, ZnO/SiO 2-entrapped materials provide twofold longer breakthrough times for H 2S (with a 67% reduction in sorbent loading) compared with packed beds of 1 to 2 mm commercial extradates. Five-log reductions in H 2S concentration with up to 75% ZnO utilization at breakthrough are achieved. H 2S concentrations from 60 to 2000 parts per million in volume (ppmv) can be reduced to as little as 0.6 ppmv at 400°C in 30% H 2O at a face velocity of 1.7 cm/s for layers as thin as 1.0 mm. At 500 to 600°C, ZnO/SiO 2-entrapped materials provide much higher regenerability in air than do 1 to 2 mm commercial extrudates. The use of glass fibers permits greater than 50 regeneration cycles.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 439-441 |
| 页数 | 3 |
| 期刊 | Journal of Materials Engineering and Performance |
| 卷 | 15 |
| 期 | 4 |
| DOI | |
| 出版状态 | 已出版 - 8月 2006 |
| 已对外发布 | 是 |
引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver