摘要
The inhibition performance of a newly synthesized thioureido imidazoline inhibitor (TAI) in CO2 corrosion was studied by using electrochemical impedance spectroscopy (EIS), atomic force microscopy (AFM) and X-ray photoelectron spectroscopy (XPS). Results show that the values of inhibition efficiency show peak-value-phenomenon at concentration of 0.15mmoldm-3 owing to the change of adsorption mode. The adsorption of protonated TAI molecules on the negatively charged steel surface makes the potential of zero charge (PZC) shift to positive direction, and the long-range electrostatic exclusive forces between AFM tip and sample surface are reduced by screening effect of surface charges.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 353-361 |
| 页数 | 9 |
| 期刊 | Corrosion Science |
| 卷 | 53 |
| 期 | 1 |
| DOI | |
| 出版状态 | 已出版 - 1月 2011 |
| 已对外发布 | 是 |
指纹
探究 'Electrochemical and surface analysis studies on corrosion inhibition of Q235 steel by imidazoline derivative against CO2 corrosion' 的科研主题。它们共同构成独一无二的指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver