We report that epitaxial strain and chemical doping can be used cooperatively to tune the sharpness of metal-insulator transition (MIT) in epitaxial (La1-xPrx)0.67Ca0.33MnO3 (LPCMO) films. Compared to multiple MITs in anisotropically strained LPCMO/(LaAlO3)0.3(SrAl0.5Ta0.5O3)0.7(001)C (LSAT) films with a phase-separated ground state, the lattice-matched LPCMO/NdGaO3(110)Or (NGO) films show a sharp MIT near the Curie temperature (TC), with a ferromagnetic-metallic ground state. The sharpness of MIT, as evaluated by the temperature coefficient of resistance (TCR), can be two times larger in LPCMO/NGO films than in LPCMO/LSAT films. Moreover, for LPCMO/NGO films, TCR greatly relies on the Pr doping level x, where a maximum TCR value of 88.17% K-1 can be obtained at x=0.25, but shows less dependence on the film thicknesses. These results suggest that the combination of epitaxial strain and chemical doping could be employed to control not only the ground state of the manganite films, but the sharpness of MIT at various TC, providing the feasibility to design manganite-based infrared devices in a broad temperature range.

源语言英语
期刊论文编号144502
期刊Journal of Applied Physics
卷116
期14
DOI
出版状态已出版 - 14 10月 2014
已对外发布是

学术指纹

探究 'Controlling the sharpness of metal-insulator transition in epitaxial (La1-xPrx)0.67Ca0.33MnO3 (0 ≤ x ≤ 0.35) films' 的科研主题。它们共同构成独一无二的学术指纹。

引用此