Abstract
With the excitation of a 978 nm laser, the upconversion (UC) emissions of the YVO4: Er3þ, Yb3þ, Cr3þ nanoparticles include three emission bands located at 524, 552 and 658 nm, respectively. The UC emission characterization confirms that the UC emission of the YVO4: Er3þ, Yb3þ nanoparticles can be modulated by the doping of the Cr3þ ions, the increase of the incident laser power and the change of the laser pulse-width. With the doping of the Cr3þ ions, the two green emissions decrease because of the energy transfer from the Er3þ states 2H11∕2 and 4S3∕2 to the Cr3þ ions. With the increase of the incident laser power, the two green emissions increase due to the decrease of the transfer rate of the energy transfer path to the state 4F9∕2 of the Er3þ ions. With the increase of the incident laser pulse-width from 0.2 to 6 ms the intensity ratio of the emission at 524 nm to the emission at 658 nm increases from 0.063 to 0.19, which is due to the number accumulation at the state 2H11∕2 due to the small transfer rate from the Er3þ state 2H11∕2 to the Cr3þ ions. The experimental results confirm that the concentration of the Cr3þ ions has less effect on the average life-time of the UC emissions at 524, 552, and 658 nm.
| Original language | English |
|---|---|
| Article number | 037106 |
| Journal | Optical Engineering |
| Volume | 63 |
| Issue number | 3 |
| DOIs | |
| State | Published - 1 Mar 2024 |
Keywords
- color modulation
- lanthanide ions
- upconversion
Fingerprint
Dive into the research topics of 'Upconversion emission and its color modulation of the YVO4: Er3+, Yb3+, Cr3+ nanoparticles'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver