Abstract
Sb2Se3, an earth-abundant, environmentally benign photovoltaic absorber, is constrained by interfacial defects, particularly at the CdS buffer layer prepared by chemical bath deposition. Conventional high-temperature (∼400 °C) CdCl2 treatment, while effective, induces detrimental deep Cd2+ diffusion. Here, we develop a low-thermal-budget hydrothermal post-treatment involving CdCl2 at 120 °C followed by a brief 200 °C activation. This strategy synergistically passivates interfacial defects: Cd2+ fills cadmium vacancies (VCd) and Cl⁻ dopes the lattice, concurrently driving the CdS phase transition from cubic to high-mobility hexagonal structure. Consequently, the CdS electron mobility surges from 145.8 to 364.9 cm2 V−1 s−1, and the CdS/Sb2Se3 band alignment is optimized to a favorable spike-like configuration (+0.11 eV). The treated substrate-configurated solar cells achieve a champion power conversion efficiency of 10.49%, a 44% improvement from the 7.30% of control devices, with enhanced open-circuit voltage, short-circuit current, and fill factor. This work demonstrates a dual-passivation, low-temperature interface engineering route that suppresses defect formation while promoting carrier transport, providing a viable strategy for high-efficiency Sb2Se3 photovoltaics.
| Original language | English |
|---|---|
| Article number | 110907 |
| Journal | Results in Engineering |
| Volume | 30 |
| DOIs | |
| State | Published - Jun 2026 |
UN SDGs
This output contributes to the following UN Sustainable Development Goals (SDGs)
-
SDG 7 Affordable and Clean Energy
Keywords
- CdS defect chemistry
- First-principles defect calculations
- Interfacial defect passivation
- Low-temperature hydrothermal processing
- SbSe solar cells
Fingerprint
Dive into the research topics of 'Low-temperature hydrothermal CdCl2 interface engineering for concurrent Cd/Cl dual-passivation in efficient Sb2Se3 solar cells'. Together they form a unique fingerprint.Cite this