TY - JOUR
T1 - Catalyst-Free Growth of Two-Dimensional BCxN Materials on Dielectrics by Temperature-Dependent Plasma-Enhanced Chemical Vapor Deposition
AU - Yi, Kongyang
AU - Jin, Zhepeng
AU - Bu, Saiyu
AU - Wang, Dingguan
AU - Liu, Donghua
AU - Huang, Yamin
AU - Dong, Yemin
AU - Yuan, Qinghong
AU - Liu, Yunqi
AU - Wee, Andrew Thye Shen
AU - Wei, Dacheng
N1 - Publisher Copyright:
Copyright © 2020 American Chemical Society.
PY - 2020/7/22
Y1 - 2020/7/22
N2 - Traditional methods to prepare two-dimensional (2D) B-C-N ternary materials (BCxN), such as chemical vapor deposition (CVD), require sophisticated experimental conditions such as high temperature, delicate control of precursors, and postgrowth transfer from catalytic substrates, and the products are generally thick or bulky films without the atomically mixed phase of B-C-N, hampering practical applications of these materials. Here, for the first time, we develop a temperature-dependent plasma-enhanced chemical vapor deposition (PECVD) method to grow 2D BCxN materials directly on noncatalytic dielectrics at low temperature with high controllability. The C, N, and B compositions can be tuned by simply changing the growth temperature. Thus, the properties of the as-made materials including band gap and conductivity are modulated, which is hardly achieved by other methods. A 2D hybridized BC2N film with a mixed BC2N phase is produced, for the first time, with a band gap of about 2.3 eV. The growth temperature is 580-620 °C, much lower than that of traditional catalytic CVD for growing BCxN. The product has a p-type conducting property and can be directly applied in field-effect transistors and sensors without postgrowth transfer, showing great promise for this method in future applications.
AB - Traditional methods to prepare two-dimensional (2D) B-C-N ternary materials (BCxN), such as chemical vapor deposition (CVD), require sophisticated experimental conditions such as high temperature, delicate control of precursors, and postgrowth transfer from catalytic substrates, and the products are generally thick or bulky films without the atomically mixed phase of B-C-N, hampering practical applications of these materials. Here, for the first time, we develop a temperature-dependent plasma-enhanced chemical vapor deposition (PECVD) method to grow 2D BCxN materials directly on noncatalytic dielectrics at low temperature with high controllability. The C, N, and B compositions can be tuned by simply changing the growth temperature. Thus, the properties of the as-made materials including band gap and conductivity are modulated, which is hardly achieved by other methods. A 2D hybridized BC2N film with a mixed BC2N phase is produced, for the first time, with a band gap of about 2.3 eV. The growth temperature is 580-620 °C, much lower than that of traditional catalytic CVD for growing BCxN. The product has a p-type conducting property and can be directly applied in field-effect transistors and sensors without postgrowth transfer, showing great promise for this method in future applications.
KW - chemical sensor
KW - field-effect transistor
KW - plasma-enhanced chemical vapor deposition
KW - temperature dependent
KW - transfer-free
KW - two-dimensional BCN
UR - https://www.scopus.com/pages/publications/85088491699
U2 - 10.1021/acsami.0c08555
DO - 10.1021/acsami.0c08555
M3 - 文章
C2 - 32574487
AN - SCOPUS:85088491699
SN - 1944-8244
VL - 12
SP - 33113
EP - 33120
JO - ACS Applied Materials and Interfaces
JF - ACS Applied Materials and Interfaces
IS - 29
ER -